Friction caused an ignition on the face of longwall panel 52 as the head drum of the shearer struck a hard rock intrusion located between the main coal seam and the draw slate. The intrusion was between 16 and 18 inches long and 2-6 inches thick. A yellow colored flame appeared to be the size of a loaf of bread and was observed as it lasted about 8 seconds by the shearer operator.